Busson, C., Blin, M. .-A., Guichard, P., Soudan, P., Crosnier, O., Guyomard, D. & Lestriez, B. (2018) A primed current collector for high performance carbon-coated LiFePO4 electrodes with no carbon additive. J. Power Sources, 406 7–17.   
Last edited by: Richard Baschera 2018-12-20 09:08:05 Pop. 1.5%
Cuisinier, M., Dupre, N., Moreau, P. & Guyomard, D. (2013) NMR monitoring of electrode/electrolyte interphase in the case of air-exposed and carbon coated LiFePO4. J. Power Sources, 243 682–690.   
Added by: Laurent Cournède 2016-03-10 21:23:29 Pop. 1%
Cuisinier, M., Dupre, N., Martin, J.-F., Kanno, R. & Guyomard, D. (2013) Evolution of the LiFePO4 positive electrode interface along cycling monitored by MAS NMR. J. Power Sources, 224 50–58.   
Added by: Laurent Cournède 2016-03-10 21:23:31 Pop. 1%
Dupre, N., Martin, J.-F., Oliveri, J., Soudan, P., Yamada, A., Kanno, R. & Guyomard, D. (2011) Relationship between surface chemistry and electrochemical behavior of LiNi1/2Mn1/2O2 positive electrode in a lithium-ion battery. J. Power Sources, 196 4791–4800.   
Added by: Laurent Cournède 2016-03-10 21:32:20 Pop. 1%
Dupre, N., Martina, J.-F., Guyomard, D., Yamada, A. & Kanno, R. (2009) Characterization of interphases appearing on LiNi0.5Mn0.5O2 using Li-7 MAS NMR. J. Power Sources, 189 557–560.   
Added by: Laurent Cournède 2016-03-10 21:41:24 Pop. 1%
Dupre, N., Martin, J.-F., Oliveri, J., Guyomard, D., Yamada, A. & Kanno, R. (2008) Unique control of bulk reactivity by surface phenomena in a positive electrode of lithium battery. Electrochem. Commun. 10 1897–1900.   
Added by: Laurent Cournède 2016-03-10 21:58:40 Pop. 1%
Wang, Z., Dupre, N., Lajaunie, L., Moreau, P., Martin, J.-F., Boutafa, L., Patoux, S. & Guyomard, D. (2012) Effect of glutaric anhydride additive on the LiNi0.4Mn1.6O4 electrode/electrolyte interface evolution: A MAS NMR and TEM/EELS study. J. Power Sources, 215 170–178.   
Added by: Laurent Cournède 2016-03-10 21:28:38 Pop. 1%